DAXWAZÎ QUOTE
| Awa |
Yarn |
Tevnkirin |
Density ( 10 mm ) |
Giranî |
Stûrahî |
Firahî |
||
|
|
Warp |
Weft |
|
Warp |
Weft |
|
|
|
| JZZ01P-100 |
1k |
1k |
adî |
7.5 |
7.5 |
100 |
0.14 |
80-150 |
| JZZ01T-100 |
1k |
1k |
twill |
7.5 |
7.5 |
100 |
0.14 |
80-150 |
| JZZ01P-120 |
1k |
1k |
adî |
9 |
9 |
120 |
0.16 |
80-150 |
| JZZ01T-120 |
1k |
1k |
twill |
9 |
9 |
120 |
0.16 |
80-150 |
| JZZ01P-140 |
1k |
1k |
adî |
10.5 |
10.5 |
140 |
0.17 |
80-150 |
| JZZ01T-140 |
1k |
1k |
twill |
10.5 |
10.5 |
140 |
0.17 |
80-150 |
| JZZ01E-140 |
1k |
1k |
Satin |
12 |
12 |
160 |
0.18 |
80-150 |
| JZZ03P-180 |
3k |
3k |
adî |
4.5 |
4.5 |
180 |
0.28 |
80-150 |
| JZZ03T-180 |
3k |
3k |
twill |
4.5 |
4.5 |
180 |
0.28 |
80-150 |
| JZZ03P-200 |
3k |
3k |
adî |
5 |
5 |
200 |
0.3 |
80-150 |
| JZZ03T-200 |
3k |
3k |
twill |
5 |
5 |
200 |
0.3 |
80-150 |
| JZZ03P-240 |
3k |
3k |
adî |
6 |
6 |
240 |
0.32 |
80-150 |
| JZZ03T-240 |
3k |
3k |
twill |
6 |
6 |
240 |
0.32 |
80-150 |
| JZZ03P-280 |
3k |
3k |
adî |
7 |
7 |
280 |
0.34 |
80-150 |
| JZZ03T-280 |
3k |
3k |
twill |
7 |
7 |
280 |
0.34 |
80-150 |
| JZZ03E-320 |
3k |
3k |
Satin |
8 |
8 |
320 |
0.36 |
80-150 |
| JZZ06P-280 |
6k |
6k |
adî |
3.5 |
3.5 |
280 |
0.36 |
80-150 |
| JZZ06T-280 |
6k |
6k |
twill |
3.5 |
3.5 |
280 |
0.36 |
80-150 |
| JZZ06P-320 |
6k |
6k |
adî |
4 |
4 |
320 |
0.38 |
80-150 |
| JZZ06T-320 |
6k |
6k |
twill |
4 |
4 |
320 |
0.38 |
80-150 |
| JZZ06P-400 |
6k |
6k |
adî |
5 |
5 |
400 |
0.42 |
80-150 |
| JZZ06T-400 |
6k |
6k |
twill |
5 |
5 |
400 |
0.42 |
80-150 |
| JZZ12P-400 |
12k |
12k |
adî |
2.5 |
2.5 |
400 |
0.46 |
80-150 |
| JZZ12T-400 |
12k |
12k |
twill |
2.5 |
2.5 |
400 |
0.46 |
80-150 |
| JZZ12P-480 |
12k |
12k |
adî |
3 |
3 |
480 |
0.52 |
80-150 |
| JZZ12T-480 |
12k |
12k |
twill |
3 |
3 |
480 |
0.52 |
80-150 |
| JZZ12P-640 |
12k |
12k |
adî |
4 |
4 |
640 |
0.64 |
80-150 |
| JZZ12T-640 |
12k |
12k |
twill |
4 |
4 |
640 |
0.64 |
80-150 |
| Area Weight | 200 g/m2 | 300 g/m2 | 600 g/m2 |
| Stûrahiya Sêwirana Fabric | 0.111 mm | 0.167mm | 0.333mm |
| Tensile Strength | >= 3400 MPa | >= 3400 MPa | >= 3400 MPa |
| Modulusa Elastîk | >= 240 GPa | >= 240 GPa | >= 240 GPa |
| Break Elongation | >=1.7% | >=1.7% | >=1.7% |
| Specification Fabric |
Giraniya tevahî (g/m2) |
0° |
90° |
+45° |
-45° |
Mifteya dirûnê (g/m2) |
Binder (g/m2) |
| C-PN600-12 |
602 |
300 |
300 |
2 |
|||
| C-PN600-50 |
602 |
300 |
300 |
2 |
|||
| C-LT400-12 |
402 |
200 |
200 |
2 |
|||
| C-LT600-50 |
602 |
300 |
300 |
2 |
|||
| C-TX500-12 |
502 |
200 |
150 |
150 |
2 |
||
| C-QX600-12 |
602 |
150 |
150 |
150 |
150 |
2 |
|
| C-L150-12-B |
174 |
150 |
12 |
4 |
8 |
||
| C-P150-12-B |
176 |
150 |
10 |
8 |
8 |
||
| C-N150-12-B |
176 |
10 |
150 |
8 |
8 |
||
| C-L300-50-B |
326 |
300 |
12 |
4 |
10 |
||
| C-P300-12-B |
328 |
300 |
10 |
8 |
10 |
||
| C-N300-12-B |
328 |
10 |
300 |
8 |
10 |
||
| C-L600-50-B |
628 |
600 |
12 |
4 |
12 |
||
| C-PN260-12 |
262 |
130 |
130 |
2 |
|||
| C-LT260-12 |
262 |
130 |
130 |
2 |
|||
| C-PN400-12 |
402 |
200 |
200 |
2 |
|||
| C-QX400-12 |
402 |
100 |
100 |
100 |
100 |
2 |
JLON li seranserê hilberînê prosedurên kontrolkirina kalîteyê yên hişk dişopîne. Her beş ji bo domdariya fîberê, rastbûna tevnê, kalîteya rûkê, û performansa mekanîkî tê kontrol kirin. Pelên Daneyên Teknîkî (TDS) li ser daxwazê hene ku piştgirî bidin verastkirina materyalê.